Plastic and nonmetallic article shaping or treating: processes – Forming continuous or indefinite length work – Shaping by extrusion
Patent
1985-02-19
1988-02-16
Silbaugh, Jan H.
Plastic and nonmetallic article shaping or treating: processes
Forming continuous or indefinite length work
Shaping by extrusion
264200, 264207, 26421116, 106196, D01D 506, D01F 228
Patent
active
047253940
ABSTRACT:
High strength, high modulus cellulose triacetate fibers are produced by spinning a 30-50% by weight solution of cellulose triacetate having an acetyl content of at least 42.5% and an inherent viscosity of at least 5 from a solvent mixture comprising nitric acid and another solvent having a molecular weight of less than 160 in a mol ratio of 1-3 through an air gap into a coagulating bath.
REFERENCES:
patent: Re30352 (1980-07-01), Kwolek
patent: 1521876 (1925-01-01), Farrow
patent: 1943461 (1934-01-01), Traill et al.
patent: 4370168 (1983-01-01), Kamide et al.
patent: 4464323 (1984-08-01), O'Brien
E. I. Du Pont de Nemours and Company
Lorin Hubert C.
Silbaugh Jan H.
LandOfFree
Process for preparing high stength cellulosic fibers does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for preparing high stength cellulosic fibers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing high stength cellulosic fibers will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2219819