ABSTRACT:
A fluidized bed reactor is supplied with fuel, oxygen-containing gas, and kaolinite, which contains water of crystallization. At least 80% by weight of the kaolinite have particle sizes in the range from 0.1 to 3 mm. A fluidized bed at temperatures in the range from 850.degree. to 950.degree. C. is formed in the fluidized bed reactor. A meta-kaolin white pigment which contains water of crystallization not in excess of 2% by weight is withdrawn from the fluidized bed reactor.
REFERENCES:
patent: 3519453 (1970-07-01), Morris et al.
patent: 5011534 (1991-04-01), Berube et al.
patent: 5393340 (1995-02-01), Slepetys et al.
Bareuther Ernst
Kauper Jochen
Rahn Martin
Stockhausen Werner
Dubno Herbert
Marcheschi Michael
Metallgesellschaft Aktiengesellschaft
Myers Jonathan
LandOfFree
Process for preparing a meta-kaolin white pigment from kaolinite does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for preparing a meta-kaolin white pigment from kaolinite, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing a meta-kaolin white pigment from kaolinite will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2353563