ABSTRACT:
Disclosed is a process for making a lightweight silicate aggregate. The process includes the steps of mixing together dry rice hull ash, an alkali metal hydroxide, boric acid, and water; heating the mixture to a temperature sufficient to initiate reaction; curing the composition at a temperature less than the boiling point of water until the reaction is complete; comminuting the cured product and heating the comminuted product to form the expanded aggregate.

REFERENCES:
patent: 4308065 (1981-12-01), Walls-Muycelo

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing a lightweight expanded silicate aggregate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing a lightweight expanded silicate aggregate , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing a lightweight expanded silicate aggregate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1986961

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.