Plastic and nonmetallic article shaping or treating: processes – Outside of mold sintering or vitrifying of shaped inorganic... – Utilizing binder to add green strength to preform
Patent
1998-02-19
2000-09-05
Fiorilla, Christopher A.
Plastic and nonmetallic article shaping or treating: processes
Outside of mold sintering or vitrifying of shaped inorganic...
Utilizing binder to add green strength to preform
264669, C04B 3332
Patent
active
061138444
ABSTRACT:
The present invention relates to a method for ore pelletization including the step of adding binder polymer to particulate ore and moisture to form an intimate mixture. Green pellets are formed from the mixture and fired. A water soluble treatment polymer having a molecular weight of 1,000 to 20,000 is included in the intimate mixture in an amount of at least 0.001% by weight. The water soluble treatment polymer is formed by polymerization of water soluble ethylenically unsaturated monomer blend containing at least 50% by weight of anionic monomer.
REFERENCES:
patent: 4342599 (1982-08-01), Mann et al.
patent: 4751259 (1988-06-01), Roe et al.
patent: 5171361 (1992-12-01), Dingeman et al.
patent: 5306327 (1994-04-01), Dingeman et al.
patent: 5821283 (1998-10-01), Hesler et al.
Ciba Specialty Chemicals Water Treatments Limited
Crichton David R.
Fiorilla Christopher A.
LandOfFree
Process for pelletizing particulate materials does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for pelletizing particulate materials, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for pelletizing particulate materials will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2208955