Process for obtaining narrow molecular weight distribution in vi

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

526 83, 526 84, 526 85, C08F 240

Patent

active

047134216

ABSTRACT:
In a process for the mass polymerization of vinyl aromatic monomer wherein vinyl aromatic monomer is polymerized in successive stages of increasing temperature, the improvement which narrows the molecular weight distribution of the resulting polymer comprising incorporating a polymerization inhibiting agent into a polymerizing mass at a point where about 60 to about 95% of monomer is converted to polymer.

REFERENCES:
patent: 2225471 (1940-12-01), Foord
patent: 2563997 (1951-08-01), Elwell
patent: 3084143 (1963-04-01), Hieserman
patent: 3110706 (1963-11-01), Vollmert
patent: 3131033 (1964-04-01), Volkenburgh

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for obtaining narrow molecular weight distribution in vi does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for obtaining narrow molecular weight distribution in vi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for obtaining narrow molecular weight distribution in vi will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1220746

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.