Process for making foam using paint sludge

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Cellular products or processes of preparing a cellular...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

521 46, 5211091, 521155, C08G 1800

Patent

active

06084003&

ABSTRACT:
Paint sludge is mixed with a polyether or polyester polyol. Optionally, lignin in the range of 0.25 to 70% by weight may be mixed with polyol. The paint sludge-polyol mixture is mixed with an isocyanate for curing the material into a mass. Alternatively, the lignin-polyol-paint sludge mixture is mixed with an isocyanate for curing the material into a mass. The lignin improves the flame resistance and moisture resistance of the mass. A catalyst may be added to the mixture to improve the rate of reaction.

REFERENCES:
patent: 4303559 (1981-12-01), Trost
patent: 4472230 (1984-09-01), Sachs et al.
patent: 4661527 (1987-04-01), Seng
patent: 5352709 (1994-10-01), Tarrant et al.
patent: 5684053 (1997-11-01), Spangler
patent: 5710199 (1998-01-01), Hubert et al.
patent: 5716996 (1998-02-01), Ketterman et al.
patent: 5834529 (1998-11-01), Reesie et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for making foam using paint sludge does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for making foam using paint sludge, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making foam using paint sludge will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1487117

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.