ABSTRACT:
Mixing under low shear vinyl-containing polyorganosiloxane, a silicon-bonded hydrogen polysiloxane and a platinum catalyst, and continue mixing produces a crumb which has an extrusion rate of at least 50 grams per minute through an orifice of 0.5 inch diameter under a pressure of 345 kilopascals and compression points of less than 1035 kilopascals. The crumb is useful in hydraulic applications.

REFERENCES:
patent: 3843601 (1974-10-01), Bruner
patent: 4528156 (1985-07-01), Fukuda et al.
"Materials News from Dow Corning"/ Nov.-Dec. 1969, New Shock-Absorbing Bumper Turns 30-mph Crash into 5-mph Bump.--p. 3.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for making crumb silicone material does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for making crumb silicone material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making crumb silicone material will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-614673

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.