Process for making a flexible polyurethane foam

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Cellular products or processes of preparing a cellular...

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C521S130000, C521S137000, C521S170000

Reexamination Certificate

active

06884825

ABSTRACT:
Process for preparing a flexible polyurethane foam comprising reacting at an isocyanate index of 70 to 130, 1) 40-65 parts by weight of a polyisocyanate composition comprising a) 80-100% by weight of a diphenylmethane diisocyanate component comprising, based on 100 parts by weight of the diphenylmethane diisocyanate component, i) 75-100 parts by weight of diphenylmethane diisocyanate comprising 15-75 parts by weight of 4,4′-diphenylmethane diisocyanate, and 25 to 85 parts by weight of 2,4′-diphenylmethane diisocyanate, and 2,2′-diphenylmethane diisocyanate and/or a liquid variant of such diphenylmethane diisocyanate, and ii) 0 to 25 parts by weight of homologues of diphenylmethane diisocyanates having an isocyanate functionality of 3 or more; and b) 20-0% by weight of toluene diisocyanate; 2) 20 to 45 parts by weight of a polyether polyol having an average molecular weight of 4500-10000, an average nominal functionality of 2-6 and comprising oxypropylene and optionally oxyethylene groups, the amount of oxypropylene groups being at least 70% by weight calculated on the weight of this polyol; 3) 3 to 20 parts by weight of a polyether polyol having an average molecular weight of 700-4000, an average nominal functionality of 2-6 and an hydroxyl value of at most 225 mg KOH/g and comprising oxyethylene and optionally oxypropylene groups, the amount of oxyethylene groups being at least 70% by weight calculated on the weight of this polyol; and 4) 2-6 parts by weight of water, wherein the amount of the polyisocyanate composition, polyol 2), polyol 3), and water being 100 parts by weight.

REFERENCES:
patent: 4506040 (1985-03-01), Raes et al.
patent: 5521226 (1996-05-01), Bleys
patent: 5597885 (1997-01-01), Lutter et al.
patent: 5919395 (1999-07-01), Bastin et al.
patent: 6417241 (2002-07-01), Huygens et al.
patent: 31 25 402 (1983-01-01), None
patent: 188 766 (1986-07-01), None
patent: 418 039 (1991-03-01), None
patent: 0 418 039 (1991-03-01), None
patent: 555 721 (1993-08-01), None
patent: 0 555 721 (1993-08-01), None
patent: 2329642 (1999-03-01), None
patent: WO 9635744 (1996-11-01), None
patent: WO 0008083 (2000-02-01), None
patent: WO 0073362 (2000-12-01), None
patent: WO 0153370 (2001-07-01), None
R.D. Priester, Jr. et al., “High Resiliency Polyurea Foam—An Improved Flexible Foam Matrix”, Journal of Cellular Plastics, Mar. 1994, p. 144, vol. 30, Technomic Publishing Co., Inc.
D.R. Gier et al., “Fillers, Hard Phases and Copolymer Polyols—Their Different Mechanism to Reinforce Flexible Polyurethane Foams”, Polyurethanes Expo '98, Sep. 17-20, 1998, p. 227.
J.P. Armistead et al., “Morphology of Water-Blown Flexible Polyurethane Foams”, Journal of Applied Polymer Science, 1988, 601-629, vol. 35, John Wiley & Sons, Inc.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for making a flexible polyurethane foam does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for making a flexible polyurethane foam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making a flexible polyurethane foam will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3401221

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.