Plastic and nonmetallic article shaping or treating: processes – Including step of generating heat by friction
Patent
1991-01-31
1991-12-03
Dixon, Jr., William R.
Plastic and nonmetallic article shaping or treating: processes
Including step of generating heat by friction
264212, 26421111, 264 60, 264216, 264166, 501136, 501 88, 501 97, 501127, C04B 3564
Patent
active
050698397
ABSTRACT:
The firing shrinkage of ceramic film casting mixtures can be increased by adding a high molecular weight mixed ester or a mixture of various high molecular weight mixed esters to them. The ceramic material of the ceramic film casting mixtures is composed preferably of lead titanate, silicon carbide, silicon nitride, beryllium oxide or aluminum oxide. Preferably, the mixed esters are derived from at least one C.sub.2 -C.sub.10 -dicarboxylic acid and at least one C.sub.8 -C.sub.24 -monocarboxylic acid. The proportion of high molecular weight mixed ester in the film casting mixture amounts to up to 5% by weight, based on the proportion of solids in the casting mixture, including sintering aids.
The process makes it possible to alter the composition of a slip and still use the old tools which require an unaltered firing shrinkage.
REFERENCES:
patent: 3717487 (1973-02-01), Hurley et al.
patent: 3988405 (1976-10-01), Smith et al.
patent: 3991149 (1976-11-01), Hurwitt
patent: 4025462 (1977-05-01), Cleveland
patent: 4109377 (1978-08-01), Blazick et al.
patent: 4548879 (1985-10-01), St. John et al.
patent: 4587068 (1986-05-01), Borase et al.
patent: 4654223 (1987-03-01), Araps et al.
patent: 4670325 (1987-05-01), Bakos et al.
patent: 4816072 (1989-03-01), Harley et al.
Grote Dieter
Muller Fritz
Pavlicek Heinz
Dixon Jr. William R.
Hoechst Ceramtec Aktiengesellschaft
Marcantoni Paul
LandOfFree
Process for increasing the firing shrinkage of ceramic film cast does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for increasing the firing shrinkage of ceramic film cast, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for increasing the firing shrinkage of ceramic film cast will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1695630