ABSTRACT:
An improved silk textile is described which exhibits more desirable wet wrinkle-recovery and tear strength than untreated silk. The silk textile contains polycarboxylic acid cross-links which are relatively strong and resistant to hydrolysis.
A process for manufacturing an improved silk textile is presented which includes wetting an untreated silk textile with a specially formulated finishing agent. The finishing agent includes polycarboxylic acid, a catalyst, and a swelling agent. The wetted silk textile is dried and cured at an elevated temperature.
REFERENCES:
patent: 3630659 (1971-12-01), Hendricks et al.
patent: 3632391 (1972-01-01), Whitfield et al.
patent: 3649346 (1972-03-01), Bridgeford et al.
patent: 3881047 (1975-04-01), Massy et al.
patent: 4066392 (1978-01-01), Abel et al.
patent: 4820307 (1989-04-01), Welch et al.
patent: 4929248 (1990-05-01), Fuse et al.
patent: 4936865 (1990-06-01), Welch et al.
Texture Asia, Lee et al., vol. 22, No. 12, pp. 86-91.
S. Sundaram, The Indian Textile Journal, pp. 138-140, Some Aspects of Wet Processing of Silk, Mar. 1990.
Li Shiqi
Yang Yiqi
Bell James J.
The Board of Trustees of the University of Illinois
LandOfFree
Process for increasing the crease resistance of silk textiles does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for increasing the crease resistance of silk textiles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for increasing the crease resistance of silk textiles will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-435398