Process for improving the strength of sialon

Compositions: ceramic – Ceramic compositions – Refractory

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

501 96, 264 66, 427226, 427227, C04B 3558

Patent

active

051186462

ABSTRACT:
A process for improving the strength of components manufactured from sialon comprising heating and components at a temperature of from about 750.degree. to 950.degree. C. for from about eight to thirty-six hours in an oxygen-containing atmosphere.

REFERENCES:
patent: 4127416 (1984-10-01), Lumby et al.
patent: 4506021 (1985-03-01), Jack et al.
patent: 4558018 (1985-12-01), Matsuhiro et al.
patent: 5017530 (1991-05-01), Arakawa et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for improving the strength of sialon does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for improving the strength of sialon, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for improving the strength of sialon will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2228317

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.