ABSTRACT:
A method for making a corrosion resistant, ferritic steel alloy, with reduced magnetic coercivity is disclosed. The process includes the step of providing an intermediate form of a ferritic alloy consisting essentially of, in weight percent, about
REFERENCES:
patent: 3923560 (1975-12-01), Regitz
patent: 4244754 (1981-01-01), Masumoto et al.
patent: 4390378 (1983-06-01), Rastogi
patent: 4394192 (1983-07-01), Rastogi
patent: 4421574 (1983-12-01), Lyudkovsky
patent: 4601766 (1986-07-01), Rastogi et al.
patent: 4772341 (1988-09-01), Rastogi et al.
patent: 5091024 (1992-02-01), DeBold et al.
"Standard Specification for Low-Carbon Magnetic Iron", ASTM Designation: A 848/A848M-96 pp. 1-5 (1996).
"REMKO Soft Magnetic Iron", Technical Bulletin, Uddeholm Corporation, Totowa, NJ (1988).
Dulmaine Bradford A.
Masteller Millard S.
CRS Holdings, Inc.
Sheehan John
LandOfFree
Process for improving magnetic performance in a free-machining f does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for improving magnetic performance in a free-machining f, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for improving magnetic performance in a free-machining f will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1391227