ABSTRACT:
Alloys reacting with water, water vapor and reactive gases at temperatures in the range of about 200.degree. to about 650.degree. C have essential components of nickel, titanium an zirconium. The alloys can be made by arc melting zirconium, nickel and titanium and can be formed into sheet or foil by inert-atmosphere hot rolling. The alloys can also be made by plating nickel on a sheet of zirconium-titanium alloy and then conduction a diffusion process by heating the plated alloy in vacuum.

REFERENCES:
patent: 1151160 (1915-08-01), Brown et al.
patent: 2926981 (1960-03-01), Stout et al.
patent: 3141830 (1964-07-01), Klepfel et al.
patent: 3467493 (1969-09-01), Eguchi et al.
patent: 3535074 (1970-10-01), Nakashima

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for gettering moisture and reactive gases does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for gettering moisture and reactive gases, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for gettering moisture and reactive gases will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-724300

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.