Chemistry: electrical and wave energy – Processes and products
Patent
1979-04-25
1981-02-24
Kaplan, G. L.
Chemistry: electrical and wave energy
Processes and products
C25D 1108, C25D 1110, C25D 1114
Patent
active
042526205
ABSTRACT:
Anodized films having an aesthetic value are formed over the surface of aluminum or aluminum alloy substrates by anodizing the substrate in an electrolyte solution containing 50-60% of sulfuric acid and oxalic acid or nickel sulfate, at a bath temperature of 18.degree. to 30.degree. C. and a current density of 1 to 10 A/dm.sup.2.
The oxide film formed by this method has a porcelain-like texture or feel or the appearance of a meshwork thereof or a grainy texture resembling wood, leather or sand, depending upon the nature of the base or substrate metal and the anodizing conditions employed.
REFERENCES:
patent: 2963409 (1960-12-01), Ramirez
LandOfFree
Process for forming an anodized film over the surface of aluminu does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for forming an anodized film over the surface of aluminu, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for forming an anodized film over the surface of aluminu will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1407713