ABSTRACT:
A process for forming a titanium base alloy comprises compacting a powder formed of particles of titanium or of a mother alloy thereof and of a dispersion of fine particles of a product curbing the growth of the grain size, in a proportion per volume which is less than that which would lead to the formation of a continuous layer of fine particles about the particles of titanium powder. Then the alloy is heat treated at a temperature higher than the point of transformation into phase .beta. and quenched. The product is typically selected among S, P, B, As, Se, Te, Y and the lanthanides.

REFERENCES:
patent: 3181947 (1965-05-01), Vordahl
patent: 4134758 (1979-01-01), Nagai et al.
patent: 4219357 (1980-08-01), Yolton et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for forming a titanium base alloy with small grain size does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for forming a titanium base alloy with small grain size , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for forming a titanium base alloy with small grain size will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-865219

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.