ABSTRACT:
A component made of superalloy is provided with a localized coating formed from three layers by a brazing heat treatment, the layers comprising an outer layer having a composition adapted to the specific surface properties sought, an inner layer having a composition which includes flux elements, and an intermediate layer obtained by the deposition of a mixture of the materials used for the other two layers.

REFERENCES:
patent: 3849865 (1974-11-01), Gedwill et al.
patent: 4005988 (1977-02-01), Paulonis et al.
patent: 4117179 (1978-09-01), Jackson et al.
patent: 4705203 (1987-11-01), McComas et al.
patent: 5021629 (1991-06-01), Shimomura
patent: 5236116 (1993-08-01), Solanki et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for forming a coating on a superalloy component, and the does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for forming a coating on a superalloy component, and the, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for forming a coating on a superalloy component, and the will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1986271

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.