Metal treatment – Process of modifying or maintaining internal physical... – Carburizing or nitriding using externally supplied carbon or...
Reexamination Certificate
2006-04-18
2008-10-21
La Villa, Michael (Department: 1794)
Metal treatment
Process of modifying or maintaining internal physical...
Carburizing or nitriding using externally supplied carbon or...
C148S212000, C148S228000, C148S231000, C148S238000, C148S317000, C427S376600, C427S383300, C427S436000
Reexamination Certificate
active
07438769
ABSTRACT:
A method for diffusing titanium and nitride into a base material having a coating thereon using conventional surface treatments or coatings. The method generally includes the steps of providing a base material having a coating thereon; providing a salt bath which includes sodium dioxide and a salt selected from the group consisting of sodium cyanate and potassium cyanate; dispersing metallic titanium formed by electrolysis of a titanium compound in the bath; heating the salt bath to a temperature ranging from about 430° C. to about 670° C.; and soaking the base material in the salt bath for a time of from about 10 minutes to about 24 hours. In accordance with another aspect of the present invention, titanium and nitride may be diffused into a base material without a coating. The treated base material may further be treated with conventional surface treatments or coatings.
REFERENCES:
patent: 3639641 (1972-02-01), Saton
patent: 4019928 (1977-04-01), Beyer et al.
patent: 4332653 (1982-06-01), Satoh
patent: 4492604 (1985-01-01), Muller et al.
patent: 6645566 (2003-11-01), Ko
patent: 6881498 (2005-04-01), Cooper et al.
Ko Bongsub Samuel
Ko Philos Jongho
Cummings Eugene M.
La Villa Michael
LandOfFree
Process for diffusing titanium and nitride into a material... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for diffusing titanium and nitride into a material..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for diffusing titanium and nitride into a material... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3995568