ABSTRACT:
A process for degreasing ceramic molded bodies containing a large quantity of paraffin wax includes a constant-temperature heating conducted for a certain period of time appropriately determined according to the size and shape of the ceramic molded bodies, at a temperature immediately below the temperature for the ceramic molded bodies to begin contraction, essentially in a low temperature region wherein the contraction occurs due to liquefaction of the paraffin wax and optionally in a high temperature region wherein the contraction occurs due to thermal decomposition of the paraffin wax. According to the process of the invention, build-up of stress in the ceramic molded bodies by heating is prevented and a temperature gradient between the surface and the inside of the molded bodies is leveled, so that crack-free molded bodies are obtained with a shortened degreasing schedule.
REFERENCES:
patent: 4704242 (1987-11-01), Bandyopadhyay
patent: 4713206 (1987-12-01), Matsuhisa et al.
patent: 4923652 (1990-05-01), Murakawa
patent: 5021208 (1991-06-01), Ludwig
Soviet Inventions Illustrated, Section Ch, Week C42, Nov. 26, 1980, Derwent Publications Ltd.
Derwent Accession No. 87-139 575, Questel Telesystems (WPIL), Derwent Publications Ltd.
Derwent Accession No. 84-278 269, Questel Telesystems (WIPL), Derwent Publications Ltd.
Adachi Masakazu
Imao Kouichi
Derrington James
NGK Insulators Ltd.
LandOfFree
Process for degreasing ceramic molded bodies does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for degreasing ceramic molded bodies, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for degreasing ceramic molded bodies will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1503525