ABSTRACT:
Dealuminizing cast iron by contacting it with free-flowing flux particles having a solid silica core and a molten silica shell wherein said flux comprises silica and about 1% to about 5% calcium fluoride.
REFERENCES:
patent: 2306976 (1942-12-01), Pedersen
patent: 2694023 (1954-11-01), Hopkins
patent: 3320052 (1967-05-01), Bowden
patent: 3446614 (1969-05-01), Johnson
patent: 3617259 (1971-11-01), Doliwa
patent: 3998624 (1976-12-01), Harris et al.
patent: 4040818 (1977-08-01), Clegg
patent: 5078784 (1992-01-01), Craig
Katz Seymour
Tiwari Basant L.
General Motors Corporation
Plant Lawrence B.
Rosenberg Peter D.
LandOfFree
Process for dealuminizing molten cast iron does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for dealuminizing molten cast iron, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for dealuminizing molten cast iron will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-696071