ABSTRACT:
Large-sized calcium nitrate tetrahydrate particles are obtained by dissolving phosphate rock in concentrated nitric acid, cooling the resulting solution, intentionally terminating the crystallization of the calcium nitrate tetrahydrate when only 40 to at most 60% of the calcium in solution has been crystallized, to form a mother liquor, recovering a portion of the mother liquor equivalent to 20 to 80% of the solution by removing the calcium nitrate crystals therefrom; combining the remainder of the suspension with the separated mother liquor and recovering the crystals with a particle size of from 70 to 1100 microns.
REFERENCES:
patent: 1816285 (1931-07-01), Johnson
patent: 1939351 (1933-12-01), Johnson
patent: 2252280 (1941-08-01), Balz
patent: 2609271 (1952-09-01), Plusje
patent: 2813777 (1957-11-01), Swenson
patent: 3205062 (1965-09-01), Gattiker et al.
Moldovan Iuliu Virgil Florian
Suciu Maria
Tomescu Eugenia
Dubno Herbert
Institutul de Cercetari Chimice - Icechim
Ross Karl F.
Turk Arnold
Wolk Morris O.
LandOfFree
Process for crystallizing calcium nitrate does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for crystallizing calcium nitrate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for crystallizing calcium nitrate will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1438046