Solid material comminution or disintegration – Processes – With heating or cooling of material
Patent
1976-05-12
1977-09-06
Lindsay, Jr., Robert L.
Solid material comminution or disintegration
Processes
With heating or cooling of material
65 19, 75 24, 75 30, 75 63, 75 72, 209 3, 209 11, 241 24, 266137, 266232, B02C 2310, C03B 1700
Patent
active
040463230
ABSTRACT:
A process for controlled slow cooling of non-ferrous smelting slags, such as copper slags, for the recovery of the non-ferrous metals contained therein by subsequent crushing, milling and flotation operations is disclosed. The process comprises the steps of pouring the molten slag into a ladle, allowing the slag to slowly cool and solidify in the ladle at least to the point where a shell is formed which is strong enough to withstand dumping from the ladle, dumping the slag from the ladle in a single piece, allowing the dumped slag to cool until its center is substantially solidified, and breaking the dumped slag in small pieces for further cooling, crushing, milling and flotation operations. Alternatively, the top of the slag in the ladle may be water cooled while the slag is allowed to slowly cool in the ladle until its center is substantially solidified. The slag is then dumped and subsequently broken in small pieces.
REFERENCES:
patent: 1402363 (1922-01-01), Hurst
patent: 2798048 (1957-07-01), Magri et al.
McKerrow George C.
Newman Christopher J.
Pelletier Albert
Lindsay, Jr. Robert L.
Noranda Mines Limited
LandOfFree
Process for controlled slow cooling of non-ferrous smelting slag does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for controlled slow cooling of non-ferrous smelting slag, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for controlled slow cooling of non-ferrous smelting slag will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2159184