ABSTRACT:
In accordance with the present invention, a process for coating a titanium or titanium alloy golf club head is presented, wherein a brazing composition is securely adhered to the titanium or titanium alloy golf club head, preferably on the striking surface thereof. The brazing composition is disposed on the titanium striking surface and the golf club head is subjected to a vacuum furnace process. The vacuum process of the present invention is designed so that the brazing composition including the plurality of hard particles is securely bonded to the titanium striking surface to form a hard, durable striking surface on the golf club head.
REFERENCES:
patent: 3736995 (1973-06-01), Salter
patent: 3989861 (1976-11-01), Rasmussen
patent: 4768787 (1988-09-01), Shira
patent: 4917384 (1990-04-01), Caiati
patent: 4951953 (1990-08-01), Kim
patent: 5207427 (1993-05-01), Saeki
patent: 5407202 (1995-04-01), Igarashi
patent: 5620382 (1997-04-01), Cho et al.
patent: 5851158 (1998-12-01), Winrow et al.
Barr Michael
Beck Shrive
PureSpin Golf Company, Inc.
LandOfFree
Process for coating a titanium golf club head and manufacture of does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for coating a titanium golf club head and manufacture of, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for coating a titanium golf club head and manufacture of will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2254531