ABSTRACT:
A process for coating a steel strip, particularly ferritic stainless steel, with aluminum by hot quenching, in which the strip is preheated to a temperature less than 500.degree. C. in a first non-oxidizing atmosphere containing a quantity of oxygen less than 3%, the strip is then heated to a temperature less than 950.degree. C. in a second non-oxidizing atmosphere, the strip is then conveyed to an atmosphere (3, 4) which is non-reactive at the coating temperature, and, finally, the strip is quenched in a coating bath.
REFERENCES:
patent: Re29726 (1978-08-01), Byrd et al.
patent: 2926103 (1990-02-01), Brick
patent: 3320085 (1967-05-01), Turner, Jr.
patent: 3925579 (1975-12-01), Flinchum et al.
patent: 4053663 (1977-10-01), Caldwell et al.
patent: 4140552 (1979-02-01), Arnold et al.
patent: 4144379 (1979-03-01), Patil et al.
patent: 4584211 (1986-04-01), Higuchi et al.
patent: 4591395 (1986-05-01), Steele, Jr. et al.
patent: 4675214 (1987-06-01), Kilbane et al.
patent: 4913785 (1990-04-01), Uchida et al.
patent: 5023113 (1991-06-01), Boston et al.
Baroux Bernard
Brun Charles G.
Buscarlet Eric
de Veyrac Patrice
Hennechart Jean-Paul
Owens Terry J.
Sollac
Ugine, Aciers de Chatillon & Gueugnon
LandOfFree
Process for coating a ferritic stainless steel strip with alumin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for coating a ferritic stainless steel strip with alumin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for coating a ferritic stainless steel strip with alumin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-133859