ABSTRACT:
A procedure based on suspension smelting has been developed for producing lead bullion from sulphidic concentrates in which the proportion of iron and of slag-forming substances is low. In the procedure oxygen or oxygen-enriched air is used. The slag containing lead oxide that is formed is in equilibrium with the sulphur-containing but refinable lead bullion. The lead oxide content of the slag may be lowered without increasing the sulphur content of the lead bullion by regulating the temperature, the FeO+CaO/SiO.sub.2 ratio and the degree of oxidation. In order that the highest possible amount of the lead contained in the concentrate might be recovered from the settler (3), the quantity of lead compounds in the gas phase is minimized and a hot cyclone is used in the uptake shaft (4) of the smelting furnace.

REFERENCES:
patent: 3847595 (1974-11-01), Liang

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Procedure for producing lead bullion from sulphide concentrate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Procedure for producing lead bullion from sulphide concentrate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Procedure for producing lead bullion from sulphide concentrate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-112729

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.