ABSTRACT:
The prevention of lithium clusters from bridging between the negative and positive portions of a cell during discharge is described. This is done by limiting the amount of electrolyte in the cell, thereby eliminating excess electrolyte pooling above the cell stack. It is in this excess electrolyte that a relatively higher Li+ion concentration can occur, creating an anodically polarized region resulting in the reduction of lithium ions on the negative and positive surfaces as the concentration gradient is relaxed. Typically, a lithium ion concentration gradient sufficient to cause lithium cluster formation is induced by the high rate, intermittent discharge of a lithium/silver vanadium oxide (Li/SVO) cell.
REFERENCES:
patent: 4209576 (1980-06-01), Heurtel
patent: 4310609 (1982-01-01), Liang et al.
patent: 4391729 (1983-07-01), Liang et al.
patent: 4830940 (1989-05-01), Keister et al.
patent: 5435874 (1995-07-01), Takeuchi et al.
patent: 5472810 (1995-12-01), Takeuchi et al.
patent: 5516340 (1996-05-01), Takeuchi et al.
patent: 5545497 (1996-08-01), Takeuchi et al.
patent: 5571640 (1996-11-01), Takeuchi et al.
patent: 5695892 (1997-12-01), Leising et al.
patent: 5716422 (1998-02-01), Muffoletto et al.
patent: 5716735 (1998-02-01), Muffoletto et al.
patent: 6221534 (2001-04-01), Takeuchi et al.
patent: 6413669 (2002-07-01), Takeuchi et al.
patent: 6451483 (2002-09-01), Probst et al.
patent: 6558845 (2003-05-01), Leising et al.
patent: 6566007 (2003-05-01), Takeuchi et al.
patent: 6685752 (2004-02-01), Leising et al.
patent: 6696201 (2004-02-01), Leising et al.
patent: 6797017 (2004-09-01), Leising et al.
patent: 7005214 (2006-02-01), Takeuchi et al.
patent: 7068036 (2006-06-01), Syracuse et al.
Takeuchi, Esther S. and Thiebolt III, William C. Lithium Deposition in Prismatic Lithium Cells During Intermittent Discharge. J. Electrochem. Soc., vol. 138, No. 9, Sep. 1991.
Leising Randolph
Palazzo Marcus
Takeuchi Esther S.
Greatbatch Ltd.
Kalafut Stephen J.
Scalise Michael F.
LandOfFree
Prevention of lithium deposition in nonaqueous electrolyte... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Prevention of lithium deposition in nonaqueous electrolyte..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Prevention of lithium deposition in nonaqueous electrolyte... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3989130