ABSTRACT:
Production of boron-containing steel slabs free from surface defects by continuous casting, particularly prevention of the slab surface crackings by cooling the slab with a specific cooling rate through the temperature range from the melting point to 900.degree. C. so as to prevent boron-containing compounds such as BN from precipitating along the austenite grain boundary. Great advantage over the conventional art is that boron-containing molten steels which could not be continuously cast can be successfully continuously cast into slabs free from surface defects.
Miyamura Kou
Ohno Yasuhide
Suzuki Hiroo
Yamamoto Koichi
Hampilos Gus T.
Lin K. Y.
Nippon Steel Corporation
LandOfFree
Prevention of cracking of continuously cast steel slabs containi does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Prevention of cracking of continuously cast steel slabs containi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Prevention of cracking of continuously cast steel slabs containi will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-936244