Chemistry: electrical and wave energy – Processes and products
Patent
1981-07-13
1983-11-01
Kaplan, G. L.
Chemistry: electrical and wave energy
Processes and products
204 32R, C25D 534
Patent
active
044128924
ABSTRACT:
Process for activating surfaces of superalloys and stainless steels prior to electroplating a metal such as chromium thereon, whereby a metal deposit having excellent adhesion to the substrate is obtained. The article is activated by anodic etching in a novel activation solution containing about 55% to 80% by volume of H.sub.2 SO.sub.4 and about 1% to 10% by volume of commercial 52% hydrofluoric acid, preferably an aqueous bath containing 65% by volume of 95-98% H.sub.2 SO.sub.4 and 5% by volume of 52% hydrofluoric acid at 30 A/dm.sup.2 and 20.degree. C. for one minute.
REFERENCES:
patent: 2044742 (1936-06-01), Armstrong et al.
patent: 3287237 (1966-11-01), Wilton
Metal Finishing Guide Book and Directory 1978, Metals and Plastics Publicons, Inc., Hackensack, N.J., pp. 202-204.
Baldauf William
Chen Edward S.
Erkkila A. Victor
Gibson Robert P.
Kaplan G. L.
Lane Anthony T.
Leader William
LandOfFree
Pretreatment of superalloys and stainless steels for electroplat does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Pretreatment of superalloys and stainless steels for electroplat, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pretreatment of superalloys and stainless steels for electroplat will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2167651