ABSTRACT:
A method of pressure leaching nickel and cobalt from sulphidic precipitates is provided, wherein such precipitates are leached with chlorine at a controlled redox potential of between 400 and 550 mV (Ag/AgCl), catalysed by copper, and at a temperature of between 120.degree. and 160.degree. C., to dissolve at least 80% of cobalt and to oxidize less than 10% of sulphur to sulphate.
REFERENCES:
patent: 3880653 (1975-04-01), Hougen
patent: 4062924 (1977-12-01), Glaum
patent: 4304664 (1981-12-01), Victorovich et al.
patent: 4377410 (1983-03-01), Thomas
patent: 4828809 (1989-05-01), Thomassen et al.
patent: 4927794 (1990-05-01), Marcantonio
Dunn Ronald R.
Xue Tao
Gorgos Kathryn
Mee Brendan
Primak George J.
LandOfFree
Pressure leaching of nickel and cobalt sulphides with chlorine u does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Pressure leaching of nickel and cobalt sulphides with chlorine u, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pressure leaching of nickel and cobalt sulphides with chlorine u will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2321966