ABSTRACT:
Unwanted recrystallization during heat treatment of a directionally solidified nickel alloy single crystal casting is prevented by chemical milling the part before heat treatment. Removal of a layer of as little as 0.013-0.050 mm thick, less than two percent of the part thickness, has been found effective.

REFERENCES:
patent: 3057764 (1962-10-01), La Boda et al.
patent: 3494709 (1970-02-01), Piearcey
patent: 3576070 (1971-04-01), Parsons
patent: 3873512 (1975-03-01), Latanision
patent: 4116723 (1978-09-01), Gell et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4345950 (1982-08-01), O'Hara

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of single crystal superalloys for post-casting heat does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of single crystal superalloys for post-casting heat , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of single crystal superalloys for post-casting heat will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1702498

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.