Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Polymers from only ethylenic monomers or processes of...
Reexamination Certificate
2005-01-18
2005-01-18
Choi, Ling-Siu (Department: 1713)
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Polymers from only ethylenic monomers or processes of...
C526S064000, C526S352000
Reexamination Certificate
active
06844408
ABSTRACT:
Ethylene homopolymers and copolymers are prepared in a tube reactor at from 160° C. to 350° C. and pressures in the range from 500 to 5000 bar, with or without use of molar mass regulators, using a peroxide mixture comprising from 1 to 95 mol %, based on the total amount of the peroxide mixture, of at least one cyclic peroxide of the formula I,where the radicals R are identical or different and are selected from among alkyl groups and aryl groups, as polymerization initiator.
REFERENCES:
patent: 4135044 (1979-01-01), Beals
patent: 4175169 (1979-11-01), Beals et al.
patent: 5376739 (1994-12-01), Pfleger et al.
patent: 5907022 (1999-05-01), Stigter et al.
patent: 0 121 755 (1984-10-01), None
patent: 0 573 870 (1993-12-01), None
patent: 0 813 550 (1997-12-01), None
patent: WO 0001740 (2000-01-01), None
Dröge Thomas
Fischer Ernst
Gonioukh Andrei
Klimesch Roger
Köhler Gernot
Basell Polyolefine GmbH
Choi Ling-Siu
Keil & Weinkauf
LandOfFree
Preparation of polyethylene does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Preparation of polyethylene, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of polyethylene will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3436606