ABSTRACT:
Mixtures of high molecular weight polyisobutylene and thermoplastic polymers are prepared in an extruder by a process in which meterable, high molecular weight polyisobutylene is first metered into the extruder and homogenized in at least one kneading stage, heated and subjected to controlled molecular weight degradation and the thermoplastic polymer is then introduced into the polyisobutylene melt by means of a side feed and is subsequently homogenized together with said melt. The novel process is particularly suitable for the preparation of mixtures of high molecualr weight polyisobutylene and polyethylene.
REFERENCES:
patent: 2339958 (1944-01-01), Sparks
patent: 3230288 (1966-01-01), Henderson
patent: 4155655 (1979-05-01), Chiselko et al.
patent: 4352823 (1982-10-01), Cherukuri et al.
patent: 4892911 (1990-01-01), Genske
Ullmann's Encyclopedia, vol. A 21, 4 pp. 555-562, 1992.
Brosius Sibylle
Fauth Karl-Heinz
Hofmann Jurgen
Kessler Thomas
Marczinke Bernd Lothar
BASF - Aktiengesellschaft
Weber Thomas R.
LandOfFree
Preparation of mixtures of high molecular weight polyisobutylene does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Preparation of mixtures of high molecular weight polyisobutylene, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of mixtures of high molecular weight polyisobutylene will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-343080