Preparation of linear .alpha.-olefin polymers having ultra high

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Polymers from only ethylenic monomers or processes of...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

526153, 526159, 526352, 526905, C08F11002

Patent

active

039843874

ABSTRACT:
Ultra high molecular weight, linear .alpha.-olefin polymers are produced without reactor fouling by polymerizing an .alpha.-olefin in the presence of Ziegler catalyst dispersed in an inert diluent and an amount of an inert gas not in excess of that which will dissolve in the inert liquid diluent.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of linear .alpha.-olefin polymers having ultra high does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of linear .alpha.-olefin polymers having ultra high , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of linear .alpha.-olefin polymers having ultra high will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-654372

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.