ABSTRACT:

BACKGROUND OF THE INVENTION
1. Field of the Invention
The present invention relates to a preparation method of gamma-butyrolactone (GBL) using maleic anhydride (MAN).
2. Description of the Related Art
Current marketability and fair possibility of growth considered, GBL, tetrahydrofuran (THF) and 1,4-butanediol (BDO) are most intriguing substances in the aspect of the industry. A major use of GBL is as a solvent or an intermediate for the pharmaceutical industry. GBL is also used as a feedstock for the production of pyrrolidone, which is used as a solvent for many industrial applications, and a substitute feedstock for pyrrolidone.
The hydrogenation of MAN is comprised of a series of reaction steps. The first step is hydrogenating the double bond (C═C) of MAN to form succinic anhydride (SA) and the subsequent one is hydrogenating the C═O group to yield GBL and THF. The secondary product of the reaction, BDO is directly manufactured from THF, GBL and SA. Byproducts with a chain structure, including alkanes, alcohols and acids are produced from hydrogenolysis of MAN. As well known in the art, the catalytic hydrogenation of MAN leads to various hydrogenated products including SA, GBL, THF and BDO as well as relatively less valuable products such as propanol, butanol and butyric acid.
The catalytic hydrogenation of MAN to GBL is a well-established art for which a great many processes and conditions have been tried to achieve high conversion and high selectivity to GBL with keen interest. However, commercial practice in respect to the production of GBL from MAN has not been entirely successful, especially in terms of high conversion and high selectivity to GBL. These deficiencies usually result from low catalytic activity, byproducts and/or inadequate process conditions, that is, optimally high temperature and pressure.
Dunlop, in U.S. Pat. No. 3,065,243, for example, describes a process in which MAN, SA, or an acid or ester thereof is vaporized and the vapors in hydrogen pass over a reduced copper-chromite catalyst. But, the conversion and selectivity to GBL are relatively low. Kyowa, in U.K. Patent No. 1,168,220 discloses that a reduced copper-zinc-chromium catalyst can be used in place of the copper-chromite catalyst but with only marginally improved results.
Miya, in U.S. Pat. No. 3,580,930, employs a copper-zinc-chromium catalyst with an at most 50% selectivity to GBL.
Attig, in EPA 332,140, describes hydrogenation for converting MAN to THF and GBL in the presence of a copper-zinc-chromium-alumina catalyst with an at most 50% selectivity to GBL.
U.S. Pat. No. 3,312,718 discloses a conversion of SA to GBL in the presence of a Ni-based hydrogenation catalyst along with silicotungastic acid as a promoter. U.S. Pat. No. 3,113,138 discloses a conversion of SA to GBL using a palladium catalyst in the liquid phase. However, these processes adversely lead to problems in regard to short lifetime of the catalysts and low yields of the products.
Canadian Pat. No. 1,041,529 describes a liquid-phase conversion of MAN to GBL using an oxide-palladium-silica catalyst with high conversion and high selectivity to GBL. But, this process inevitably requires high temperature and high pressure, for example, 250° C. and 150 kg/cm
2
and its practice in the industry gives rise to a demand of delicate and expensive facility.
Many catalyst modifications used in hydrogenation of SA to GBL are disclosed in other patents including U.S. Pat. No. 4,620,017. However, the processes using these catalysts inevitably require a step of separating the used catalyst in order to use another fresh catalyst, since SA obtained from conversion of MAN has to be separated prior to a second hydrogenation.
In commercial operation using these and other processes, as described above, the catalysts and process conditions employed have been found to be unsatisfactory, usually because the catalyst is deactivated through tar or coke formation within a relatively short time. The short lifetime of the catalysts also makes it virtually impossible to carry on a production run for a prolonged period of time. Thus developing catalysts and process conditions to achieve high conversion to GBL in a single step under adequate process conditions is of great importance in the aspects of both technology and economy.
SUMMARY OF THE INVENTION
Accordingly, it is an object of the present invention to provide a process for effecting liquid-phase hydrogenation of MAN to GBL in high conversion and high selectivity.
It is another object of the present invention to provide a process for effecting hydrogenation with a relatively low pressure, and a novel catalyst for carrying out the hydrogenation with high catalytic activity and high selectivity.
The process of this invention is very useful in the aspect of economy because conversion of MAN to GBL can be achieved in a simple reaction step and the catalyst used is stable to the reaction, i.e., retarded in deactivation, thus prolonging the lifetime, and can be recycled several times. Examples of the suitable catalyst include activated catalysts, such as palladium-molybdenum-nickel catalyst, palladium-ruthenium-nickel catalyst, or palladium-ruthenium-nickel catalyst supported on silica having a large surface area.
The present invention is directed to a liquid phase process for converting MAN to GBL in the presence of a palladium-molybdenum-nickel catalyst supported on silica that has a large surface area. The process of this invention is typically carried out at elevated temperature and pressure, for example, in the range of 100 to 275° C. and 50 to 150 kg/cm
2
, dominantly in the range of 150 to 230° C. and 50 to 100 kg/cm
2
.
FIG. 1
shows the procedure for preparing GBL. This process employs an autoclave, which is operated in a batch mode or a continuous mode. First, MAN and THF are introduced as a feedstock into the autoclave and the resulting products are separated from the catalyst to yield GBL. The GBL is then subjected to a qualitative analysis on the HPLC and GC columns.
The base material for the preparation of the catalyst is preferably a solution containing metal salts, which are soluble in water and readily decomposed in the metal form by calcination and reduction and include: nickel salts such as nickel nitrate, nickel formate, nickel acetate, or nickel salts of other volatile organic acids; palladium salts such as palladium chloride, palladium acetate, or palladium amine complex; and molybdenum salts such as ammonium molybdate tetrahydrate, molybdenum acetate, or molybdenum oxychloride.
Preferably, silica used as a carrier has a large specific surface area in the range of more than 100 to 500 m
2
/g. The use of silica whose specific surface area is less than 50 m
2
/g results in considerably low conversion and selectivity to GBL.
A sufficient amount of the catalyst is prepared from silica carrier, nickel salt solution, palladium salt solution and molybdenum salt solution with the composition as follows:
Nickel: 20-35 wt. %;
Palladium: 1-4 wt. %;
Molybdenum: 2-8 wt. %; and
Silica: for the rest in percentage
The catalysts are generally used in the form of powder or pellets. The exemplary palladium-molybdenum-nickel catalyst as used herein is supported on a carrier or in an immersion or suspension of the carrier.
In contrast to other processes for converting MAN to GBL that are conducted in the vapor phase, the process of this invention is carried out in the liquid phase which is a great advantage with regard to conversion and reactor dimensions. The liquid phase process is characterized in that the feedstock is not overheated and hence no deterioration of the catalytic activity due to coke formation. The catalytic process can be conducted in a wide range of inert solvents, for example, aromatics such as benzene, toluene or xylene; aliphatic alcohols such as methanol, ethanol or higher alcohols; dimethylformamide; and cyclic ethers such as THF or dioxane. A particularly preferred solvent for the conversion of MAN is GBL, which is the end product of the process and thus needs not be

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of gamma-butyrolactone by catalytic... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of gamma-butyrolactone by catalytic..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of gamma-butyrolactone by catalytic... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2881106

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.