ABSTRACT:
A polymerization process is provided for producing a butyl rubber with a bimodal molecular weight distribution which comprises introducing isobutylene, a conjugated diolefin monomer having from 4 to 8 carbon atoms, from about 1.times.10.sup.-5 to about 1.times.10.sup.-3 moles of an initiator component per mole of isobutylene, said initiator component being selected from the group consisting of an initiator component having the formula: ##STR1## in which R.sub.1, R.sub.2 and R.sub.3 are selected from the group consisting of alkyl, aryl and aralkyl groups and can be the same or different and i is a positive whole number from 2 to 6, and an initiator component having an adamantyl nucleus bearing from 2 to 4 hydroxyl groups an inert organic solvent and from about 1.times.10.sup.-4 to about 1.times.10.sup.-3 moles of water per liter of inert organic solvent into a suitable reaction vessel at a temperature of from about -120.degree. C. to about -50.degree. C., adding a solution of from about 5.times.10.sup.-5 to about 1.times.10.sup.-2 moles of a Lewis acid per mole of isobutylene in an organic solvent and polymerizing the monomers to form said butyl rubber.

REFERENCES:
patent: 2781334 (1957-02-01), Welch et al.
patent: 4942210 (1990-07-01), Kuntz
patent: 5071913 (1991-12-01), Powers et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of butyl rubber with bimodal molecular weight distri does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of butyl rubber with bimodal molecular weight distri, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of butyl rubber with bimodal molecular weight distri will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-351295

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.