ABSTRACT:
A granular explosive is obtained by mixing porous prill ammonium nitrate having an average particle size of 0.5 to 3.0 mm with a liquid aromatic dinitro compound and optionally a metal powder. Explosives having high sensitivity and power can be obtained by a simple and easy process.

REFERENCES:
patent: 2220891 (1940-11-01), Cook et al.
patent: 3722410 (1973-03-01), Hurst
patent: 3773573 (1973-11-01), Slykhouse
patent: 3937296 (1976-02-01), Larson
patent: 4015526 (1977-04-01), Bond et al.
patent: 4084993 (1978-04-01), Cook
patent: 4084995 (1978-04-01), Samuelsen et al.
patent: 4093478 (1978-06-01), Hurst
patent: 4334939 (1982-06-01), Bushman

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of AN-DNT-Al explosive does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of AN-DNT-Al explosive, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of AN-DNT-Al explosive will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-959936

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.