Alloys or metallic compositions – Nickel base – Chromium containing
Patent
1989-03-02
1990-09-18
Dean, R.
Alloys or metallic compositions
Nickel base
Chromium containing
148 3, 148 203, 148162, 148410, C22C 1905
Patent
active
049577034
ABSTRACT:
A precipitation-hardenable nickel-base superalloy with improved mechanical properties in the temperature range from 600.degree. to 750.degree. C. which has the following composition:
REFERENCES:
patent: 3146136 (1964-08-01), Bird et al.
Robert W. Fawley, Superalloy Progress, The Superalloys, p. 3-29, edited by Chester T. Sims and William C. Hagel, New York, 1972.
Michio Yamazaki, 1986, pp. 945-953, Proceedings of a Conference Held in Liege Belgium, 6-9, Oct. 1986.
Lawrence Peter
Nazmy Mohamed
Staubli Markus
Asea Brown Boveri Ltd.
Dean R.
LandOfFree
Precipitation-hardenable nickel-base superalloy with improved me does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Precipitation-hardenable nickel-base superalloy with improved me, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Precipitation-hardenable nickel-base superalloy with improved me will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1571469