ABSTRACT:
Heat treatments are described which improve subsequent HIP treatment results of superalloy articles. The heat treatments substantially eliminate certain low melting phases which otherwise would cause problems relating to gas entrapment during a HIP process. The articles are heated to a temperature near but below the intended HIP temperature for a period of time sufficient to reduce the low melting phase.
REFERENCES:
patent: 3753790 (1973-08-01), Walker et al.
Brown Edgar E.
Hatala Robert W.
Dean R.
Sohl Charles E.
United Technologies Corporation
LandOfFree
Pre-HIP heat treatment of superalloy castings does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Pre-HIP heat treatment of superalloy castings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pre-HIP heat treatment of superalloy castings will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2397317