ABSTRACT:
A compacted powdered iron core utilizes iron powder in the 0.002 to 0.006 mean particle size range which is first coated with an alkali metal silicate and then overcoated with a silicone resin polymer. The treated powder is compressed to approximately 94% of theoretical density and then annealed at approximately 600.degree. C. This results in a core component characterized by overall core losses as low as in conventional laminated cores in A.C. operation.
REFERENCES:
patent: 3245841 (1966-04-01), Clarke et al.
patent: 3725521 (1973-04-01), Ebling
patent: 3917976 (1975-11-01), Nuckolls
patent: 4177089 (1979-12-01), Bankson
patent: 4227166 (1980-10-01), Tsuji et al.
Soileau Trasimond A.
Speaker Lawrence W.
General Electric Company
Policinski Henry J.
Sheehan John P.
LandOfFree
Powdered iron core magnetic devices does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Powdered iron core magnetic devices, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Powdered iron core magnetic devices will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-864503