ABSTRACT:
A method to increase the fracture resistance of titanium alloy matrix composites which comprises thermally treating a composite at a temperature about 5 to 10% above the beta-transus temperature of the alloy for about 4 to 60 minutes.

REFERENCES:
patent: 4675964 (1987-06-01), Allison
patent: 4816347 (1989-03-01), Rosenthal et al.
patent: 4975125 (1990-12-01), Chakrabarti et al.
patent: 5026520 (1991-06-01), Bhowal et al.
patent: 5074907 (1991-12-01), Amato et al.
patent: 5125986 (1992-06-01), Kimura et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Post-consolidation method for increasing the fracture resistance does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Post-consolidation method for increasing the fracture resistance, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Post-consolidation method for increasing the fracture resistance will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2267446

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.