Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...
Patent
1978-11-06
1981-01-06
Henderson, C. A.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Mixing of two or more solid polymers; mixing of solid...
260 174R, 525326, 525329, 526273, 526287, C08F 836
Patent
active
042437725
ABSTRACT:
A two step process for the preparation of polymers which contain an easily controllable amount of sulfonate groups. In the first step, a copolymerization or a graft copolymerization is carried out using a controlled amount of an epoxy group containing monomer, said monomer being an ester of 2,3-epoxy propyl alcohol and acrylic acid. In a second step, the epoxy groups of the polymer prepared in the first step are, via ring opening reaction, partially or fully sulfonated by means of sulfite ions in aqueous solution in the presence of a quaternary ammonium salt as a catalyst.
REFERENCES:
patent: 3541059 (1970-11-01), Schaper
patent: 3579565 (1971-05-01), Zaslowsky
patent: 3784525 (1974-06-01), Baumann
patent: 3852256 (1974-12-01), Parker
Paul Swaraj
Ranby Bengt
LandOfFree
Polymers with controlled sulfonic acid or sulfonate group conten does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Polymers with controlled sulfonic acid or sulfonate group conten, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Polymers with controlled sulfonic acid or sulfonate group conten will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-285915