ABSTRACT:
By carefully adjusting the molecular weight and amounts of methacrylic acid and maleic acid and/or maleic anhydride comonomers in polyacrylic acid-based fiberglass binders, binder-treated fiberglass cured and B-staged product throughput may be maintained at production rates designed for phenol/formaldehyde binders due to the lower thermal requirements for cure as compared to homopolyacrylic acid-based binder systems.

REFERENCES:
patent: 3658772 (1972-04-01), Volk et al.
patent: 4076691 (1978-02-01), Swift et al.
patent: 5108798 (1992-04-01), Guerro et al.
patent: 5143582 (1992-09-01), Arkens et al.
patent: 5318990 (1994-06-01), Strauss
patent: 5412026 (1995-05-01), Holy et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Polycarboxy polymer acid binders having reduced cure temperature does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Polycarboxy polymer acid binders having reduced cure temperature, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Polycarboxy polymer acid binders having reduced cure temperature will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-850164

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.