ABSTRACT:
Avoidance of the corrosion initiation sites consisting of Mn particles deposited on the TiG welded inner tube surface is achieved through suppression of emission of manganese fumes by addition of a protective non corrosive metallic layer. The latter melts during the welding and arises in a non-corrosive internal metallic coating of the welded zone.
REFERENCES:
patent: 385384 (1888-07-01), Thomson
patent: 2850798 (1958-09-01), Bowman et al.
"Arc Welding of Stainless Steel", Metals Handbook, 8th Edition, vol. 6, Aug. 1971, pp. 251-2.
Boireau Alain
Chevrel Henri
Bradley P. Austin
Knapp Jeffrey T.
L'Air Liquide Societe Anonyme pour l'Etude et, l'Exploitation de
Wittenberg Malcolm B.
LandOfFree
Pipe welding process using a metallic insert for improved corros does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Pipe welding process using a metallic insert for improved corros, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pipe welding process using a metallic insert for improved corros will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-68985