ABSTRACT:
A permanent magnet essentially consisting of in weight percent, 60% to 68% at least one transition element by weight, 30% to 38% at least one rare earth element by weight, 0.1% to 1.5% nitrogen by weight, and 0.8% to 1.5% boron by weight is disclosed. A method for producing the permanent magnet containing at least one rear element, at least one rare earth element, nitrogen and boron includes melting, cooling, milling, magnetizing, and compacting the transition element, the rare earth element and boron to form a green compact, and then sintering the green compact in nitrogen atmosphere having a constant partial pressure for 1 to several hours to form the permanent magnet.
REFERENCES:
patent: 3970484 (1976-07-01), Doser
patent: 4601875 (1986-07-01), Yamamoto et al.
patent: 4888512 (1989-12-01), Shimizu
patent: 4902357 (1990-02-01), Imaizumi
Chin Tsung-Shune
Heh Shiang-Jiun
Lin Ken-Der
High End Metals Corp.
Sheehan John P.
LandOfFree
Permanent magnet and the method for producing the same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Permanent magnet and the method for producing the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Permanent magnet and the method for producing the same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1931089