Permanent decrease of wood hardness by in situ polymerization of

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Polymers from only ethylenic monomers or processes of...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

427393, 427440, 428511, 428513, 428514, 428536, 4285371, 428541, B32B 2108, B05D 300

Patent

active

060638834

ABSTRACT:
A wood article is submitted to a vacuum in an autoclave to remove air that it contains. Then, a solution which contains a water-soluble cross-linkable prepolymer, a polymerization initiator and optionally a wood preservative is introduced into the autoclave. Polymerization to form a polymeric network in the wood article is carried out in an atmosphere which may be substantially free of oxygen, while the optionally present preservative is chemically fixed to the wood. The result is a wood article with a permanently reduced hardness and an increased moisture content at equilibrium.

REFERENCES:
patent: 5731096 (1998-03-01), Besner

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Permanent decrease of wood hardness by in situ polymerization of does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Permanent decrease of wood hardness by in situ polymerization of, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Permanent decrease of wood hardness by in situ polymerization of will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-259741

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.