ABSTRACT:
Active material for a positive electrode of a rechargeable alkaline electrochemical cell is made with nickel hydroxide particles or cobalt-coated nickel hydroxide particles treated with strongly oxidizing reagents such as alkali metal persulfate in alkaline solution. The active material also may be made with cobalt-coated nickel hydroxide particles having a high percentage of cobalt(III) on a surface or an average cobalt oxidation state of about 3 measured across the particles. The treated nickel hydroxide or cobalt-coated nickel hydroxide decreases the cobalt solubility in the alkaline electrolyte and increases the high-rate charge and discharge capability. The lower cobalt solubility decreases cobalt migration that can increase self discharge and lead to premature failure.

REFERENCES:
patent: 3647544 (1972-03-01), Schneider
patent: 3870564 (1975-03-01), Takamura et al.
patent: 3951687 (1976-04-01), Takamura et al.
patent: 3961985 (1976-06-01), Takamura et al.
patent: 4003754 (1977-01-01), Winsel et al.
patent: 4017665 (1977-04-01), Sandera et al.
patent: 5215836 (1993-06-01), Eisenberg
patent: 5523182 (1996-06-01), Ovshinsky et al.
patent: 5804334 (1998-09-01), Yamamura
patent: 5968684 (1999-10-01), Hayashi et al.
patent: 6040007 (2000-03-01), Junichi et al.
patent: 6225004 (2001-05-01), Hayashi
patent: 6436575 (2002-08-01), Weckesser et al.
patent: 6617072 (2003-09-01), Venkatesan et al.
patent: 6649305 (2003-11-01), Bugnet et al.
patent: 6787265 (2004-09-01), Phillips
patent: 7261972 (2007-08-01), Inada et al.
patent: 7829221 (2010-11-01), Phillips
patent: 2002/0037455 (2002-03-01), Tani et al.
patent: 2002/0172758 (2002-11-01), Nanno et al.
patent: 2003/0140483 (2003-07-01), Wakabayashi et al.
patent: 2004/0115533 (2004-06-01), Phillips
patent: 2005/0003270 (2005-01-01), Phillips
patent: 2006/0029863 (2006-02-01), Miyamoto et al.
patent: 2009/0208839 (2009-08-01), Geng et al.
patent: 0833397 (1976-04-01), None
patent: 0457354 (1991-11-01), None
patent: 0697746 (1996-02-01), None
patent: 0 902 490 (1999-03-01), None
patent: 1 172 869 (2002-01-01), None
patent: 1207576 (2002-05-01), None
patent: 1 367 666 (2003-12-01), None
patent: 1 699 099 (2006-09-01), None
patent: 902490 (2008-11-01), None
patent: 1168471 (2011-01-01), None
patent: 54163324 (1979-12-01), None
patent: 56-29345 (1981-07-01), None
patent: 07037609 (1995-02-01), None
patent: 11297352 (1999-10-01), None
patent: 200058062 (2000-02-01), None
patent: 2005 056 733 (2005-03-01), None
Ohta et al., “Nicel Hydroxide Electrode: Improvement of Charge Efficiency at High Temperature,” The Electrochemical Society Proceedings, vol. 94-27, pp. 296-302, 1994.
Canada Office Action dated Apr. 30, 2008, from corresponding Canadian Patent Application No. 2,325,640.
International Search Report mailed Apr. 29, 2002, PCT Application PCT/UCA01/01717.
Japan Office Action dated Feb. 22, 2008, from corresponding Japan Patent Application No. 2002-541747, with English explanation from Japanese Associate of Office Action.
Japan Abstract, dated Feb. 25, 2000, from Japan Patent Application No. 2002-058062.
Office Action dated Dec. 10, 2007 for U.S. Appl. No. 10/899,593.
Final Office Action dated Apr. 11, 2008 for U.S. Appl. No. 10/899,593.
Office Action dated Jun. 30, 2008 for U.S. Appl. No. 10/899,593.
“WordNet Search.” WordNet. Dec. 3, 2008. <http://wordnet.princeton.edu/perl/webwn?s=embedded>.
“WordNet Search.” WordNet. Dec. 3, 2008. <http://wordnet.princeton.edu/perl/webwn?s=paste>.
“WordNet Search.” WordNet. Apr. 4, 2008. <http://wordnet.princeton.edu>.
Office Action dated Dec. 4, 2008 for U.S. Appl. No. 10/899,593.
Office Action dated Mar. 6, 2009 for U.S. Appl. No. 10/899,593.
CA Office Action dated Apr. 14, 2009, from CA Appl. No. 2,325,640.
EP Office Action dated Dec. 2, 2009, from EP Appl. No. 01993957.8.
JP Office Action dated Sep. 8, 2009, from JP Appl. No. 2002-541747, with English explanation from Japanese Associate of Office Action.
US Notice of Allowance dated Nov. 19, 2009, from related U.S. Appl. No. 10/899,593.
US Notice of Allowance dated Feb. 2, 2009, from related U.S. Appl. No. 10/899,593.
U.S. Appl. No. 10/899,593, filed Jul. 26, 2004.
Search Report and Written Opinion dated May 13, 2009 for corresponding PCT Application No. PCT/US2009/033265.
Ying et al., “Surface modification of nickel hydroxide particles by micro-sized cobalt oxide hydroxide and properties as electrode materials,”Surface and Coatings Technology, Elsevier, Amsterdam, NL, vol. 200, No. 7, (Dec. 21, 2005), pp. 2376-2379, XP005181204.
Search Report and Written Opinion dated Jun. 22, 2010 for PCT Application No. PCT/US2010/033023.
US Notice of Allowance dated Jun. 14, 2010, from related U.S. Appl. No. 10/899,593.
US Notice of Allowance dated Sep. 23, 2010, from related U.S. Appl. No. 10/899,593.
US Office Action dated Apr. 5, 2011 issued in U.S. Appl. No. 12/432,639.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Pasted nickel hydroxide electrode for rechargeable... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Pasted nickel hydroxide electrode for rechargeable..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pasted nickel hydroxide electrode for rechargeable... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4265536

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.