Passivating metals on cracking catalysts

Compositions – Preservative agents – Anti-oxidants or chemical change inhibitants

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

252437, 252456, 208120, B01J 2702, B01J 2714

Patent

active

041418581

ABSTRACT:
Metals such as nickel, vanadium and iron contaminating a cracking catalyst are passivated by contacting the cracking catalyst under elevated temperature conditions with antimony selenide, antimony sulfide, antimony sulfate, bismuth selenide, bismuth sulfide, or bismuth phosphate.

REFERENCES:
patent: 2645605 (1953-07-01), Lang et al.
patent: 3417157 (1968-12-01), Pollitzer
patent: 3711422 (1973-01-01), Johnson et al.
patent: 3977963 (1976-08-01), Readal et al.
patent: 4025458 (1977-05-01), McKay

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Passivating metals on cracking catalysts does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Passivating metals on cracking catalysts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Passivating metals on cracking catalysts will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-721924

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.