Metal treatment – Stock – Nickel base
Patent
1989-01-11
1991-02-26
Dean, R.
Metal treatment
Stock
Nickel base
148 115N, 420443, C22C 1905
Patent
active
049959220
ABSTRACT:
Oxide-dispersion-hardened superalloy based on nickel, which is composed of the following main constituents:
REFERENCES:
patent: 4386976 (1983-06-01), Benn et al.
patent: 4668312 (1987-05-01), Benn et al.
G. H. Gessinger, Powder Metallurgy of Superalloys, Butterworths London, 1984.
R. F. Singer, et al., Conf. Proc., "High Temperature Materials for Gas Turbines", Liege, Belgium, Oct. 1986, pp. 1-30.
J. S. Benjamin, Metallurgical Transactions, vol. 1, Oct. 1970, pp. 2943-2951.
K. Mino, et al., Transaction of the Iron and Steel Institute of Japan, vol. 27, pp. 823-829, Tokyo, 1987.
M. A. Burke, et al., Scripta Metallurgica, vol. 18, pp. 91-94, Pergamon 1984.
Asea Brown Boveri Ltd.
Dean R.
LandOfFree
Oxide-dispersion-hardened superalloy based on nickel does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Oxide-dispersion-hardened superalloy based on nickel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oxide-dispersion-hardened superalloy based on nickel will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-292368