ABSTRACT:
Single crystal superalloy castings are described which have excellent oxidation resistance. The oxidation resistance is due to the presence of small but effective amounts of magnesium in the casting. Single crystal castings containing magnesium in the range of 5-200 parts per million, by weight, are described.
REFERENCES:
patent: 3146136 (1964-08-01), Bird et al.
patent: 3166412 (1965-01-01), Bieber
patent: 3859060 (1975-01-01), Eiselstein et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 5069873 (1991-12-01), Harris et al.
patent: 5335717 (1994-08-01), Chin et al.
Superalloys, edited by C. T. Sims et al: p. 293 1987.
The Making, Shaping and Treating of Steel, edited by H. E. McGannon; pp. 365 and 587 1975.
Bornstein Norman S.
Chin Stephen
Duhl David N.
Parille Donald R.
Shah Dilip M.
United Technologies Corporation
Yee Deborah
LandOfFree
Oxidation resistant single crystal superalloy castings does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Oxidation resistant single crystal superalloy castings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oxidation resistant single crystal superalloy castings will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1655704