Alloys or metallic compositions – Containing over 50 per cent metal but no base metal – Iron containing
Patent
1994-04-13
1995-04-04
Yee, Deborah
Alloys or metallic compositions
Containing over 50 per cent metal but no base metal
Iron containing
420447, 420448, 420586, C22C 3000
Patent
active
054035473
ABSTRACT:
An oxidation resistant alloy containing iron, cobalt, nickel and at least 4 to 5% by weight aluminum having at least a duplex crystalline structure. One crystalline component of this structure is a gamma (fcc) phase having a gamma prime phase dispersed therein. The second crystalline component is enriched in aluminum compared to the first crystalline component and exhibits characteristics under X-ray diffraction and electron diffraction analysis of a BCC B2 structured phase.
REFERENCES:
patent: 4066447 (1978-01-01), Smith, Jr. et al.
patent: 4144102 (1979-03-01), Smith, Jr. et al.
patent: 4642145 (1987-02-01), Masumoto et al.
patent: 4853298 (1989-08-01), Harner et al.
Taiwanese Alloy Publication, pp. 503-505, 524 & 525 Jul. 20, 1980.
Super Alloys, Special-Duty Materials, 1081 Metal Progress, vol. 122, No. 1, (1982), pp. 66-67.
Inone et al., "Microstructure and mechanical properties of rapidly quenched L2.sub.0 and L2.sub.0 +L1.sub.2 alloys in Ni-Al-Fe and Ni-Al-Co systems," Journal of Materials Science, 19, (1984) pp. 3097-3106.
Field et al., "Deformation of a Ni-Al-Fe Gamma/Beta Alloy," High Temperature Ordered Intermetallic Alloys III Symposium, (1988), pp. 567-572.
A. W. Cochardt, "High Damping Ferromagnetic Alloys",--Oct. 1956, Journal of Metals, pp. 1295-1298.
H. Masumoto, "On the Thermal Expansion of Alloys of Cobalt, Iron and Chromium, and a New Alloy `Stainless-Invar`" Science Reports, Tohoku Imperial University, 23, 1934, pp. 265-280.
H. Masumoto, "On the Thermal Expansion of the Alloys of Iron, Nickel, and Cobalt, and the Cause of the Small Expansibility of Alloys of the Invar Type" Science Reports, Tohoku Imperial University, 20, 1931, pp. 101-123.
H. Masumoto, "On the Intensity of Magnetization in Iron-Nickel-Cobalt Alloys", Science Reports, Tohoku Imperial University, 18, 1929, pp. 195-229.
H. Masumoto, "On the Coefficient of Thermal Expansion in Nickel-Cobalt and Iron-Cobalt Alloys, and the Magnetostriction of Iron-Nickel Alloys" Science Reports, Tohoku Imperial University, 16, 1927, pp. 333-341.
H. Masumoto, "On a New Transformation of Cobalt and the Equilibrium Diagrams of Nickel-Cobalt and Iron Cobalt" Science Reports, Tohoku Imperial University, 15, 1926, pp. 449-477.
Fisher Roneldo L.
Heck Karl A.
Smith John S.
Smith, Jr. Darrell F.
Biederman Blake T.
INCO Alloys International, Inc.
Steen Edward A.
Yee Deborah
LandOfFree
Oxidation resistant low expansion superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Oxidation resistant low expansion superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oxidation resistant low expansion superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2379261