Stock material or miscellaneous articles – All metal or with adjacent metals – Composite; i.e. – plural – adjacent – spatially distinct metal...
Patent
1978-06-16
1980-12-02
Rutledge, L. Dewayne
Stock material or miscellaneous articles
All metal or with adjacent metals
Composite; i.e., plural, adjacent, spatially distinct metal...
75170, 75171, 428652, 428653, 428679, B32B 1520
Patent
active
042371937
ABSTRACT:
An article of manufacture having improved high temperature oxidation and corrosion resistance comprising: (a) a superalloy substrate containing a carbide reinforcing phase, and (b) a coating consisting of chromium, aluminum, carbon, at least one element selected from iron, cobalt or nickel, and optionally an element selected from yttrium or the rare earth elements.
REFERENCES:
patent: 3573963 (1971-04-01), Maxwell
patent: 3754898 (1973-08-01), McGurty
patent: 3873347 (1975-03-01), Walker et al.
patent: 4003765 (1977-01-01), Davidson
patent: 4082581 (1978-04-01), Ghosh
Jackson Melvin R.
Rairden, III John R.
Cohen Joseph T.
Davis Jr. James C.
General Electric Company
Rutledge L. Dewayne
Saba W. G.
LandOfFree
Oxidation corrosion resistant superalloys and coatings does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Oxidation corrosion resistant superalloys and coatings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oxidation corrosion resistant superalloys and coatings will most certainly appreciate the feedback.